stiff paper coated with powdered emery or sand

References in periodicals archive ?
Lightly smooth the cut edges with emery paper and treat them with beeswax; wipe clean.
The sample should move laterally across the emery paper at a rate of 4.20 mm +0.04 mm per revolution of the drum (refs.
Designations Parameters O [beta] solution treated specimens ground by emery paper to 1000 mesh S Ground specimens cathodic charged in 1N [H.sub.2]S[O.sub.4(aq)] at 5 A/[cm.sup.2] for 15 h A Ground specimens cathodic charged in 1 N [H.sub.2]S[O.sub.4(aq)] + 0.005 M [As.sub.2][O.sub.3] at 5 A/[cm.sup.2] for 15 h T Ground specimens cathodic charged in 1 N [H.sub.2]S[O.sub.4(aq)] + 0.01 M thiourea at 5 A/[cm.sup.2] for 15 h Table 4: Designations and the associated parameters of the cyclic hydrogenation-solution treatments.
Once dry the fragile dried clay pot is refined by scraping blemishes with a small sharp knife or filed down with fine emery paper. The dry clay pot is then fired to biscuit.
Finally use emery paper or silicon carbide stone to smooth the cut end.
Begin by using emery paper to clean the area of pipe either side of the damaged bit, so as to ensure the putty is given the best chance of sticking.
The new specialty sheeter can sheet abrasive materials such as emery paper and sand papers of 25 grit or higher.
If they do get dirty and corroded, clean them with a piece of rolled up emery paper, about an inch long.
Clean the outside of the pipe with plumber's sandcloth or emery paper. Brush flux onto all four cleaned surfaces.
Remove any rust with a scouring pad or emery paper.
After filing, jewelry objects should be robbed with emery paper to remove file marks, burrs and scratches.
The shimstock can be used like emery paper and can be cut with scissors to the desired size.
It's way wise to run it against emery paper to polish the fool out of the piece before even its first use.
* Sand the outer 1 1/2 inches of the underside of the cover with emery paper.